Abstract Preview

This document specifies testing conditions for use when constructing a forming-limit curve (FLC) at ambient temperature and using linear strain paths. The material considered is flat, metallic and of thickness between 0,3 mm and 4 mm.

NOTE The limitation in thickness of up to 4 mm is proposed, giving a maximum allowable thickness to the punch diameter ratio.


General information

  • Status :  Published
    Publication date : 2021-02
  • Edition : 2
    Number of pages : 27
  • :
    ISO/TC 164/SC 2
    Ductility testing
  • 77.040.10
    Mechanical testing of metals