This document specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths.

Formula (1), on which conversions are based, is considered to be reliable when applied to austenitic stainless steels within the tensile strength range 450 to 750 N/mm2 and in the solution treated condition.

These conversions are not applicable to:

a) cold reduced steels;

b) quenched and tempered steels;

c) non-austenitic steels.

These conversions are not applicable when the gauge length exceeds  or where the width to thickness ratio of the test piece exceeds 20.


Общая информация

  • Текущий статус :  Published
    Дата публикации : 2021-12
  • Версия : 2
  • :
    ISO/TC 17/SC 20
    General technical delivery conditions, sampling and mechanical testing methods
  • 77.040.10
    Mechanical testing of metals

Цели в области устойчивого развития

Данный стандарт разработан для достижения следующих Цель устойчивого развития:

Приобрести данный стандарт

Формат Язык
PDF + ePub
Бумажный
  • CHF138

Жизненный цикл


Появились вопросы?

Ознакомьтесь с FAQ

Работа с клиентами
+41 22 749 08 88

Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)

Будьте в курсе актуальных новостей ИСО

Подписывайтесь на наши новости, обзоры, а также на информацию о продуктах.