This document specifies a method for the determination of the resistance of moulded test specimens of polypropylene and propylene-copolymers to accelerated ageing by heat in the presence of air using a forced draught oven.

The method represents an attempt to estimate the service life of parts fabricated from propylene plastics.

The stability determined by this method is not directly related to the suitability of the material for use when different environmental conditions prevail.

NOTE The specified thermal levels are considered sufficiently severe to cause failure of commercial grades of heat-stable propylene plastics within a reasonable period of time. If desired, lower temperatures can be applied to estimate the performance of propylene plastics with lower heat stabilities.


Общая информация

  • Текущий статус :  Published
    Дата публикации : 2019-07
  • Версия : 2
    Число страниц : 7
  • :
    ISO/TC 61/SC 9
    Thermoplastic materials
  • 83.080.20
    Thermoplastic materials

Приобрести данный стандарт

Формат Язык
PDF + ePub
Бумажный
  • CHF58

Жизненны цикл

Стандарт, который пересматривается каждые 5 лет



Изменения / Исправления

Появились вопросы?

Ознакомьтесь с FAQ

Работа с клиентами
+41 22 749 08 88

Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)

Будьте в курсе актуальных новостей ИСО

Подписывайтесь на наши новости, обзоры, а также на информацию о продуктах