The test can be used to determine whether cold slug or unfused areas are present, to determine the amount of moulded-in stress produced by the moulding process, reveal contamination and to show the quality of the weld. Complete fittings are subjected to a temperature of 150° centigrade in an air-circulating oven for a given time depending on the wall thickness of the fitting. The surfaces of the fitting are examined before and after heating. Cracks, blisters,*delamination or weld opening is measured, expressed as a percentage of the wall thickness.


Общая информация

  • Текущий статус :  Withdrawn
    Дата публикации : 1990-11
  • Версия : 2
    Число страниц : 3
  • :
    ISO/TC 138/SC 5
    General properties of pipes, fittings and valves of plastic materials and their accessories -- Test methods and basic specifications
  • 23.040.45
    Plastics fittings

Жизненны цикл

Стандарт, который пересматривается каждые 5 лет



Изменения / Исправления

Появились вопросы?

Ознакомьтесь с FAQ

Работа с клиентами
+41 22 749 08 88

Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)

Будьте в курсе актуальных новостей ИСО

Подписывайтесь на наши новости, обзоры, а также на информацию о продуктах