ISO 18352:2009 specifies a method for determining the residual compression strength of multidirectional polymer matrix composite laminate plates that have been damaged by impact prior to the application of in-plane compressive loading.

The test method is suitable for continuous-fibre-reinforced polymer matrix composites. Application of the method is limited to fibre-reinforced plastic laminates with multidirectional reinforcements manufactured from unidirectional prepreg tapes/fabrics or woven fabrics.

The test method is referred to as the compression-after-impact (CAI) test when used to determine the residual compression strength of an impacted plate. It can be used to obtain data for material specification, material evaluation, research and development, or construction of a composite database.


Общая информация

  • Текущий статус :  Published
    Дата публикации : 2009-08
  • Версия : 1
  • :
    ISO/TC 61/SC 13
    Composites and reinforcement fibres
  • 83.120
    Reinforced plastics

Приобрести данный стандарт

Формат Язык
PDF
Бумажный
  • CHF118

Жизненный цикл


Появились вопросы?

Ознакомьтесь с FAQ

Работа с клиентами
+41 22 749 08 88

Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)

Будьте в курсе актуальных новостей ИСО

Подписывайтесь на наши новости, обзоры, а также на информацию о продуктах.