ISO 18352:2009 specifies a method for determining the residual compression strength of multidirectional polymer matrix composite laminate plates that have been damaged by impact prior to the application of in-plane compressive loading.

The test method is suitable for continuous-fibre-reinforced polymer matrix composites. Application of the method is limited to fibre-reinforced plastic laminates with multidirectional reinforcements manufactured from unidirectional prepreg tapes/fabrics or woven fabrics.

The test method is referred to as the compression-after-impact (CAI) test when used to determine the residual compression strength of an impacted plate. It can be used to obtain data for material specification, material evaluation, research and development, or construction of a composite database.


Informations générales

  • État actuel :  Publiée
    Date de publication : 2009-08
  • Edition : 1
  • :
    ISO/TC 61/SC 13
    Composites et fibres de renforcement
  • 83.120
    Plastiques renforcés

Acheter cette norme

Format Langue
PDF
Papier
  • CHF118

Cycle de vie


Vous avez une question?

Consulter notre FAQ

Service à la clientèle
+41 22 749 08 88

Horaires d’ouverture:
De lundi à vendredi - 09:00-12:00, 14:00-17:00 (UTC+1)

Suivez l'actualité de l'ISO

Inscrivez-vous à notre Newsletter (en anglais) pour suivre nos actualités, points de vue et informations sur nos produits.